Battery Manufacturing Equipment
EQUIPMENT • CELL ASSEMBLY

Gelon laboratory post-formation pouch degassing vacuum sealer

Gelon's laboratory degassing sealer works on pouch cells after formation. It punctures the gas pocket, collects the excess electrolyte and makes the final vacuum seal. Heating reaches 250°C, sealing time adjusts from 0 to 99 seconds and the seal edge is 5 mm wide. It suits labs and pilot lines finishing small batches of formed pouch cells.

By Gelon Lib Group Co., Ltd.

BatteryEquip editorial teamSource review: 2026-10-11Buying guide based on the maker's published data.
PUBLISHED REFERENCE

Puncture, collect, seal

The machine pierces the air or gas bag, recycles the excess electrolyte and then vacuum seals the pouch. Gelon lists heating up to 250°C, sealing time from 0 to 99 seconds and a 5 mm seal edge. Compressed air is 0.5–0.8 MPa, and the supply comes as AC220 V/50 Hz or 110 V/60 Hz; name the version you need.

Cell size range, gas pocket geometry, vacuum range, heating uniformity and pressing force are not listed. The 0.5–0.8 MPa figure is the air supply, so ask separately for the vacuum level and the force at the seal. Request the chamber, fixture and seal head drawing. Edge trimming and OCV testing are done on larger finishing lines.

Original parameter values · 4 entries
ParameterPublished valueRecord status
Maximum listed heating temperature250 °Cknown
Adjustable sealing time0–99 sknown
Listed seal edge width5 mmknown
Compressed-air range0.5–0.8 MPaknown

Catalogue values apply to the configuration and test method the maker states. Ask for the values that apply to your configuration.

Source references: s1

BUYER NOTES

Where the gas and electrolyte go

Describe the state of the formed cell, the electrolyte and where the gas pocket should be opened. Ask for the puncture method, collection path, wetted materials and cleaning access. Gelon says excess electrolyte is recycled; ask how much is collected and treat any reuse as your own decision after testing.

Define how the cell is held and how much movement the body and tabs can take. Ask how the machine tells a correctly placed pouch from one that should not be punctured, since no sensing or interlock is listed. Run the demonstration with your gas pocket drawing, your cells and your planned collection procedure.

Source references: s1

BUYER NOTES

Build a seal recipe for your laminate

Agree how temperature is measured, the dwell, the force and the vacuum reference for your laminate. Set the seal position, the final pouch shape and the inspection that proves integrity. Seal strength and leak tightness have to be tested on your film. If residual gas or leak rate is part of acceptance, write down the test method.

Seal a run of cells, interrupt one cycle, then clean and change over. Find out which loading, puncture and unloading steps are manual and how an unfinished cell is set aside. Expect to measure cycle time yourself, as none is listed. At handover you should have a proven recipe and a record of seals that passed.

Gelon's profile lists the filling and sealing machines used before formation, and the formation and capacity grading page explains where the gas comes from.

Source references: s1

MAKE A SELECTION

Questions that change the purchase

DecisionWhat the catalogue saysNext step
Does the gas pocket fit the actual fixture?The page lists puncture without geometry or positioning limits.Approve pouch, chamber and head drawings.
What does electrolyte recovery mean?The page says excess electrolyte is recycled, with no method or quantity.Define collection, compatibility and cleaning, and test before any reuse.
How is the final seal accepted?The page lists temperature and time limits only.Qualify a laminate-specific seal and any required leak test.
FROM READING TO A BRIEF

Prepare the supplier conversation

Fill in the conditions below and ask the supplier to answer each open point in writing. Copying or downloading stays in your browser; nothing is sent.

Prepare a full project brief →

SOURCES

Sources and check dates

The maker's own pages and public records used for this page, each with the date it was checked.

s1 · Gelon laboratory post-formation pouch degassing vacuum sealer — manufacturer equipment page

Gelon · Manufacturer-origin source

Gelon's product page describing puncture, electrolyte recovery and vacuum sealing, with heating limit, sealing time, edge width, air and power.

Archived source check: 2026-10-11

s2 · Gelon official equipment portfolio

Gelon · Manufacturer-origin source

Gelon's equipment range, including pouch fillers, pre-sealers and larger degassing lines.

Archived source check: 2026-10-11

Still to confirm

  • The vacuum range and how it is measured.
  • Sealing force and the supported cell and gas pocket sizes.
  • Seal strength and leak tightness on your laminate with the proposed recipe.
  • The collection method for excess electrolyte and the cycle time per cell.
BEFORE YOU REQUEST A QUOTE

Final degassing and vacuum sealing of formed pouch cells

  1. Formed-cell pouch and gas-pocket drawing
  2. Electrolyte, puncture method and recovery collection path
  3. Vacuum reference/range and supplied pump boundary
  4. Seal temperature, dwell, force and final geometry
  5. Integrity/leak/residual-gas inspection and sample plan
  6. Voltage version, operator tasks and interrupted-cell recovery
Edit your enquiryRead the manufacturer dossier →
Analytics preferences

Usage analytics loads only with your consent. Private pages are excluded. Inquiry text and contact details are not sent to analytics.

Analytics has not been allowed.